Heat Resistant Steels

1.4841 Standards DIN X15CrNiSi25-20

Chemical Composition

% C0,15
% Si2,00
% Mn1,50
% Cr24,50
% Ni19,50

Applications

Steam boilers, thermocouples, etc.

Heat Treatment Properties

  • Stress Relief °C
    650
  • Delivery Hardness
    +A / max. 223

Sonrasındaki Mikroyapı
Austenite

Hardness

  • Austenitizing °C 
    1000-1150 
  • Cooling
    Su , Air