Stainless Mould Steels

1.4057 Standards DIN X17CrNi16-2

Chemical Composition

% C0,15-0,20
% Simax 1,00
% Mnmax 1,00
% Cr15,00-18,00
% Ni2,00-3,00

Applications

Glass molds, valve parts, piston rods, fittings, nuts and bolts, etc.

Heat Treatment Properties

  • Stress Relief °C
    630-720
  • Soft Annealing °C
    660-750
  • Delivery Hardness
    +A / max. 295

Hardness

  • Austenitizing °C 
    950-1050 
  • Cooling
    Yağ, Air

Hardness After Hardening

  • HRC
    47
Tempering °C                
HRC                