Heat Resistant Steels

1.4845 Standards DIN X12CrNi25-12

Chemical Composition

% C0,10
% Si0,50
% Mn1,50
% Cr24,50
% Ni19,50

Applications

Electrical resistors, furnaces, high temperature applications, air heaters etc.

Heat Treatment Properties

Delivery Hardness
+A / max. 192

Sonrasındaki Mikroyapı
Austenite

Hardness

  • Austenitizing °C 
    1000-1150 
  • Cooling
    Su , Air