Heat Resistant Steels

1.4885 Standards DIN X12CrNiMoNb20-15

Chemical Composition

% C0,10
% Si1,70
% Mn1,50
% Cr20,00
% Ni14,50

Applications

Heat Treatment Properties

Delivery Hardness
+A / max. 220

Sonrasındaki Mikroyapı
Austenite

Hardness

  • Austenitizing °C 
    1050-1150 
  • Cooling
    Su