Hot forming of ferrous and non-ferrous metals, punchs and in the production of plastic molds with high abrasion
Hardness
Hardness After Hardening
| Tempering °C | 100 | 200 | 300 | 400 | 500 | 555 | 600 | 650 | 700 |
| HRC | 53 | 52 | 51 | 52 | 54 | 53 | 50 | 43 | 31 |
| Tensile Strenght N/mm2 | 1845 | 1790 | 1730 | 1790 | 1910 | 1845 | 1680 | 1360 | 995 |

You can call or email us for all our new generation high performance steels.
You can download our catalog that contains material information about Birleşik Metal steels here.